Knowledge Battery Testing How do FIB milling parameters affect micro-battery function? Optimize beam current & dwell time to prevent damage.
Author avatar

Tech Team · Kintek Solution

Updated 3 months ago

How do FIB milling parameters affect micro-battery function? Optimize beam current & dwell time to prevent damage.


FIB milling parameters can determine whether an all-solid-state micro-battery remains electrochemically functional or becomes thermally damaged or internally shorted. High beam currents are useful for rapid bulk removal, but applying them during final cleaning can heat and damage solid electrolytes such as LiPON and promote redeposition between layers. Long pixel dwell times intensify local heating and redeposition, potentially eliminating the expected voltage plateau; a coarse-to-fine process using low-current, ultra-short-dwell cleaning is therefore preferred.

The key principle is to separate material removal from surface finishing: use relatively high current only for coarse milling, then use approximately 0.28 nA with about 100 ns pixel dwell time for final cleaning to limit heating, electrolyte damage, and conductive redeposition.

Why FIB Parameters Affect Electrochemical Functionality

The battery stack is vulnerable to local damage

An all-solid-state micro-battery contains closely spaced layers, commonly including a cathode, solid electrolyte, and anode or current collector. Because these layers are thin and adjacent, a small amount of FIB-induced damage or redeposited material can alter the electrical pathway through the entire cell.

Solid electrolytes such as LiPON are particularly important. Damage to the electrolyte can reduce ionic functionality, create leakage pathways, or allow electronic contact between electrodes.

FIB processing changes more than specimen geometry

FIB milling is intended to remove material, but the ion beam also transfers energy into the specimen. The resulting effects can include localized heating, amorphization, sputtered-material redeposition, and interface damage.

These effects matter electrochemically because the micro-battery is not merely being prepared for imaging. The milled structure may itself be used as a test cell, cross-sectional device, or in-situ biased specimen.

How Beam Current Changes Cell Behavior

High current improves coarse milling speed

A higher beam current increases the material-removal rate and is appropriate for removing the bulk of a specimen efficiently. The referenced process uses a current of up to approximately 2.8 nA at 30 kV for initial coarse milling.

This stage is relatively tolerant of surface damage because the affected material will subsequently be removed or refined during the cleaning step.

Excessive current during cleaning causes damage

Using a current above approximately 0.28 nA during fine surface cleaning increases the risk of localized heating and redeposition across the battery stack. In an amorphous solid electrolyte, such heating can degrade the material and alter the electrochemical response.

The critical distinction is therefore not simply “high current versus low current.” It is where in the process the current is applied: high current can be useful for bulk removal but harmful when directed at the final functional surface.

Redeposition can create an electrical short

Sputtered cathode, anode, electrolyte, or current-collector material can settle on nearby surfaces. If this redeposited material bridges otherwise separated layers, the micro-battery may develop an internal electronic short.

The electrochemical signature can be severe: instead of reaching its expected operating plateau, the device may show a near-zero-voltage response or a 0 V platform.

How Pixel Dwell Time Changes Cell Behavior

Long dwell times increase local energy deposition

Pixel dwell time is the time the ion beam remains at each scanned position. Longer dwell times concentrate more energy in a local region before the beam moves on, increasing the likelihood of thermal buildup and beam-induced material redistribution.

Dwell times in the range of 1–100 µs, including an example of 10 µs, can therefore be problematic during fine cleaning of sensitive battery layers.

Short dwell times reduce thermal accumulation

An ultra-short dwell time, such as approximately 100 ns, reduces the energy deposited at each pixel and limits local heating. It also reduces the opportunity for sputtered material to accumulate in a way that bridges adjacent layers.

Short dwell time does not eliminate all FIB damage, but it is an important part of controlling the combined thermal and redeposition effects.

Electrochemical activity can be lost

If long dwell times thermally damage the electrolyte or active interfaces, the cell may no longer behave like the original battery structure. The device can lose electrochemical activity and fail to reach its expected charging plateau.

For the cited Si/LiPON/LiCoO₂-type micro-battery configuration, preserving a stable charging plateau near 3.6 V is an indication that the processed structure has retained its intended functionality.

Why a Two-Step Milling Protocol Works

Step 1: Remove bulk material efficiently

The initial coarse-milling stage should use a relatively high current, with the cited protocol limiting it to approximately 2.8 nA. The objective is rapid removal of unwanted bulk material while avoiding unnecessary exposure of the final functional surface.

This step prioritizes throughput and geometry rather than ultimate surface quality.

Step 2: Finish with low-current cleaning

The final cleaning step should use a lower current, approximately 0.28 nA in the referenced protocol. Combining this current with an ultra-short dwell time near 100 ns limits the energy delivered to the exposed battery stack.

The cleaning stage is where electrochemical preservation becomes the dominant objective. It should remove residual debris without creating new damage or redeposition bridges.

Parameter control must be considered together

Beam current and dwell time are not independent in their practical effect. A lower current can still cause substantial local heating if the dwell time is too long, while a short dwell time cannot fully compensate for an excessively aggressive current during final cleaning.

The safest process window is therefore defined by the combination of current, dwell time, milling stage, scan strategy, and exposure of sensitive interfaces.

Understanding the Trade-offs

Higher throughput versus electrochemical preservation

High-current milling reduces preparation time and is valuable for coarse excavation. However, using it too close to the active stack can compromise the very cell intended for measurement.

A slower low-current cleaning step is usually justified when the purpose is quantitative electrochemical testing rather than only structural imaging.

Surface cleanliness versus additional ion exposure

More cleaning can remove redeposited material, but every additional pass also exposes the electrolyte and interfaces to the ion beam. Over-cleaning can therefore introduce additional amorphization, heating, or compositional modification.

The goal is not maximum milling. It is the minimum controlled cleaning needed to obtain a representative, electrically isolated structure.

Voltage plateau as evidence, not proof

A stable voltage plateau near the expected value, such as 3.6 V in the cited configuration, supports the conclusion that the micro-cell remains functional. Conversely, a 0 V response strongly suggests a short or severe failure.

Electrochemical behavior should still be interpreted alongside microscopy and electrical inspection, because a normal-looking cross-section does not by itself prove that interfaces and ionic pathways are undamaged.

Parameter values are process-specific

The cited values—approximately 2.8 nA for coarse milling, 0.28 nA for cleaning, and 100 ns dwell time—should be treated as a validated starting protocol for the referenced type of specimen, not universal limits for every FIB instrument or battery architecture.

Actual safe values depend on ion species, accelerating voltage, beam diameter, layer thickness, scan pattern, exposed area, and the thermal and electrical design of the specimen.

How to Apply This to Your Project

A practical workflow should validate both the physical cross-section and the post-milling electrochemical response.

  • If your primary focus is rapid bulk removal: Use a higher current, up to the validated coarse-milling limit such as approximately 2.8 nA, while keeping the beam away from the final functional interfaces as long as possible.
  • If your primary focus is preserving electrochemical activity: Perform final cleaning near 0.28 nA with an ultra-short dwell time around 100 ns, then verify that the cell retains its expected voltage plateau.
  • If your primary focus is preventing internal shorts: Minimize high-current exposure during finishing and inspect for redeposited material that could bridge cathode, electrolyte, and anode layers.
  • If your primary focus is reliable comparative data: Keep FIB parameters consistent across specimens and record current, dwell time, voltage, milling sequence, and scan conditions with each electrochemical measurement.
  • If your primary focus is diagnosing a failed micro-cell: Treat a 0 V platform or loss of the normal plateau as evidence of possible redeposition, electrolyte damage, or beam-induced interface failure rather than automatically as intrinsic battery behavior.

Careful separation of coarse milling from low-energy final cleaning allows FIB-prepared micro-batteries to remain representative electrochemical test structures rather than artifacts of specimen preparation.

Summary Table:

Parameter High Value Low Value
Beam current (coarse milling) Up to ~2.8 nA for fast removal Not recommended for final cleaning
Beam current (cleaning) Risk of heating and redeposition ~0.28 nA to preserve functionality
Pixel dwell time ~1-100 µs (e.g., 10 µs) increases damage ~100 ns to reduce thermal effects
Effect on battery Can cause short (0 V) or loss of plateau Retains voltage plateau near expected value

Ensure your battery R&D precision with KINTEK's advanced laboratory equipment. Our FIB-compatible tools and comprehensive solutions for solid-state battery fabrication help you achieve the exacting standards needed for reliable electrochemical testing. From slurry mixing to cell assembly, our portfolio supports your entire workflow. Contact us today to optimize your micro-battery preparation and avoid FIB-induced failures. Get in touch with our experts.


Leave Your Message