Electrode Slitter
50mm to 600mm Aluminum Plastic Film Slitting and Cutting Machine
Item Number : FQ05
Price varies based on specs and customizations
- Slitting Width
- Minimum 50 mm--600 mm
- Slitting Accuracy
- +/-0.5 mm
- Maximum Loading Width
- 600 mm
Shipping:
Contact us to get shipping details Enjoy On-time Dispatch Guarantee.
Why Choose Us
Easy ordering process, quality products, and dedicated support for your business success.
Product Overview


This system is designed for longitudinal slitting and roll cutting of aluminum plastic film used for soft-pack lithium battery packaging. It processes a full-width roll up to 600 mm wide through blade-based longitudinal cutting, then uses two motor-synchronized winding rollers to rewind the separated material. The result is aluminum plastic film prepared to the required production-process width with controlled handling from feed through collection.
The equipment is suited to battery R&D lines, pouch-cell pilot production, and manufacturing processes that need to divide wide aluminum plastic film into narrower packaging-film strips. Its minimum slitting width of 50 mm supports a broad practical range of cut formats, while the eight blade sets provide the cutting configuration required for multi-strip processing from one loaded roll.
A variable-frequency motor and winding motor form the primary control arrangement, providing stable control performance with adjustable operating speed. A high-power motor drives the knife roller, while the active speed-regulation winding arrangement is intended to maintain material-strip tension. Adjustable tension and cutting-roll speed give operators direct control over material handling conditions when preparing film for demanding battery packaging workflows.
Key Features
-
50 mm to 600 mm Slitting Range: The equipment slits aluminum plastic film from a minimum width of 50 mm up to 600 mm. This range supports the conversion of full-width material rolls into packaging-film widths required by the production process.
-
Longitudinal Blade Cutting: Eight blade sets perform longitudinal slitting after the roll is loaded. The cutting arrangement is built around a knife roller driven by a high-power motor to support controlled separation of the film into multiple strips.
-
Specified Cutting Accuracy: The system provides a slitting accuracy of +/-0.5 mm. This defined accuracy helps production teams control the resulting film width when preparing material for soft-pack lithium battery packaging.
-
Synchronized Dual-Roller Rewinding: Two winding rollers are synchronously driven by motors after longitudinal cutting. This coordinated collection arrangement rewinds the separated film strips following the selected cutting width.
-
Adjustable Material Tension: Tension can be adjusted from 0 to 25 N according to actual operating conditions. The active winding arrangement is configured to keep the material strip under controlled tension during the slitting and rewinding process.
-
Variable Cutting-Roll Speed: The cutting-roll speed is adjustable from 0 to 30 m/min according to actual requirements. Operators can set a suitable processing pace for the film-handling condition and production workflow.
-
Adjustable Collection Speed: Material collection speed can be adjusted according to actual conditions. This flexibility supports coordinated operation between the cutting section and the rewinding section.
-
Robust Mechanical Construction: The platform base uses 45# steel plate with a chrome-plated surface. Painted cover plates, reinforcing plates, and square-tube components form the main frame structure, while the unit also includes a safety protection plate.
-
SKD11 Slitting Blades: The slitting knives are made from SKD11 material. The blade material is specified as part of the core cutting configuration for aluminum plastic film processing.
-
Straightforward Motor-Control Arrangement: A variable-frequency motor and winding motor serve as the primary control components, with stable control performance and adjustable fast and slow operation. The system is designed for direct, convenient operation during film conversion.
Applications
| Application | Description | Key Benefit |
|---|---|---|
| Pouch Cell Packaging Film Preparation | Slits full-width aluminum plastic film into widths used in soft-pack lithium battery packaging processes. | Converts rolls up to 600 mm wide into process-ready packaging-film strips. |
| Lithium Battery R&D Lines | Prepares aluminum plastic film for research-scale soft-pack cell work where different film widths are required. | Adjustable 50 mm to 600 mm slitting width accommodates changing development requirements. |
| Battery Pilot Production | Supports controlled conversion of packaging film before downstream pouch-cell production steps. | +/-0.5 mm slitting accuracy provides a defined width-control specification. |
| Multi-Strip Film Processing | Uses eight blade sets to longitudinally divide a loaded material roll into separate film strips. | Enables multiple slit strips to be produced from a single roll-cutting operation. |
| Wide-Roll Aluminum Plastic Film Conversion | Processes rolls with a maximum loading width of 600 mm and maximum loading diameter of 350 mm. | Provides a defined capacity envelope for full-roll material preparation. |
| Tension-Sensitive Film Rewinding | Rewinds slit aluminum plastic film using two synchronously driven winding rollers and adjustable tension. | Adjustable 0 to 25 N tension supports controlled handling during collection. |
| Variable-Speed Packaging Film Cutting | Operates the knife roller at an adjustable speed of 0 to 30 m/min according to actual conditions. | Allows the processing speed to be set for the active material-handling requirement. |
Technical Specifications
| Parameter | Specification |
|---|---|
| Site-facing item identifier | FQ05 |
| Equipment function | Longitudinal slitting and roll cutting of aluminum plastic film for soft-pack lithium batteries; after blade slitting of a full roll up to 600 mm wide, two motor-synchronized winding rollers rewind the film according to the set width |
| Applicable material | Aluminum plastic film for soft-pack lithium battery packaging |
| Slitting method | Blade-based longitudinal slitting / roll cutting |
| Slitting width | Minimum 50 mm--600 mm |
| Slitting accuracy | +/-0.5 mm |
| Blade quantity | 8 sets |
| Blade material | SKD11 |
| Maximum loading width | 600 mm |
| Maximum loading diameter | 350 mm |
| Tension control | Adjustable according to actual conditions, 0-25 N |
| Cutting-roll speed | Adjustable according to actual conditions, 0-30 m/min |
| Collection speed | Adjustable according to actual conditions |
| Winding configuration | Two winding rollers synchronously driven by motors |
| Primary control components | Variable-frequency motor and winding motor |
| Knife-roller drive | High-power motor |
| Winding drive | Active winding with speed-regulation motor |
| Control characteristics | Stable control performance; adjustable fast and slow operation; convenient and intuitive operation |
| Power supply | 220V/50Hz |
| Power | 2.5KW |
| Compressed air | >=0.6MPa |
| Equipment dimensions L x W x H | Approx. 1150 x 1040 x 1040 mm |
| Frame platform base | 45# steel plate with chrome-plated surface |
| Frame structure | Painted cover plates, painted reinforcing plates, and painted square-tube main frame |
| Safety provision | Equipment safety protection plate |
| Inverter | Taichuang |
| Speed-regulation motor | Taili |
| Pneumatic components | AirATC / Xingchen |
Why Choose This Product
-
Defined Precision for Film Preparation: The specified +/-0.5 mm slitting accuracy gives procurement and process teams a clear benchmark for width control when converting aluminum plastic film for soft-pack battery packaging.
-
Capacity Matched to Full-Width Material: With a maximum loading width of 600 mm and maximum loading diameter of 350 mm, this system is configured for processing wide aluminum plastic film rolls before they are divided into narrower strips.
-
Controlled Handling from Cut to Rewind: The combination of blade slitting, two synchronized winding rollers, adjustable collection speed, and 0 to 25 N adjustable tension supports a controlled material path through the cutting and rewinding operation.
-
Specified Industrial Build Elements: A chrome-plated 45# steel plate base, reinforced painted frame construction, SKD11 blades, and an equipment safety protection plate define the mechanical configuration of the unit.
-
Practical Operating Adjustability: Adjustable cutting-roll speed from 0 to 30 m/min, adjustable tension, and variable collection speed allow the equipment to be set according to actual production conditions rather than operated at one fixed setting.
Contact us for a quote or to discuss an aluminum plastic film slitting configuration for your soft-pack lithium battery packaging process.
Trusted by Industry Leaders
Product Datasheet
50mm to 600mm Aluminum Plastic Film Slitting and Cutting Machine
REQUEST A QUOTE
Our professional team will reply to you within one business day. Please feel free to contact us!
Related Products
Automatic Film Coating Drying Machine
Automatic film coating drying machine for battery electrodes and advanced materials, with vacuum fixation, adjustable coating speed, precision thickness control, and uniform heating for reliable laboratory research and repeatable high temperature thin film preparation processes and controlled development
Small Laboratory Automatic Film Coating Drying Machine
Small laboratory automatic film coating drying machine with adjustable coating speed, precision thickness control, vacuum substrate fixation, and 130°C heated drying for battery, ceramic, crystal, and nanofilm research in glove boxes and advanced materials laboratories for consistent high temperature film preparation
200mm Roll to Roll Film Unwinding and Rewinding Machine
200mm roll to roll unwinding and rewinding machine for laboratory film processing lithium battery electrode calendaring optical films functional films continuous operation constant torque tension control with 1.5 m/min speed 50 N tension capacity and three inch cores
Small Continuous Laboratory Coating Machine for Precise Wet Film Application
Small continuous laboratory coating machine for precise wet film application supports repeatable coating of adhesives paper and films with adjustable speed and a 30 cm working width for reliable laboratory production trials and coating process development across diverse substrates
Desktop Continuous Film Coating Testing Machine for 18650 Cylindrical Batteries
Desktop continuous coating machine for lithium battery electrodes 18650 cylindrical cell research ceramic films crystal films and nanofilms offering adjustable coating width precise thickness control automatic rewinding and independent PID oven temperature regulation for university laboratories and small scale production
Coin Cell Electrode Sheet Punching Machine
Coin cell electrode sheet punching machine for precision die cutting of battery cathodes anodes separators and thin materials with compact operation flexible die sizes and glovebox compatible handling for laboratory research workflows consistent clean edges in demanding battery development applications.
Lab Manual Microtome Slicer for Tissue Sectioning
Precision Manual Slicer for labs: Achieve accurate, consistent sample preparation with adjustable high-precision cutting. Ideal for research, food, and industry.
Benchtop Slot Die Flat Plate Coater Battery Laboratory Coating Machine
Precision benchtop slot die flat plate coater and battery laboratory coating machine delivers uniform films, sealed syringe feeding, vacuum fixation, adjustable speed, controlled heating, and repeatable electrode coating for advanced research lithium ion solar polymer and OLED materials research.
Split Type Automatic Hot Press 400x600mm Platen 12kW Dual Zone Heating PID Programmable Control
Professional-grade split-type automatic hot press with large 400x600mm platen, 12kW dual-zone heating, and PID programmable temperature/pressure control. Includes water cooling for fast cycle times. Ideal for battery electrode laminating, composite panel forming, and wide film pressing.
Automatic Laboratory Unwind Rewind Machine and Unwind Rewind Device for Battery Electrodes Optical Films and Functional Materials
Automatic laboratory unwind rewind machine with servo tension control optical web guiding and split structure for lithium battery electrodes optical films and functional roll materials delivering accurate continuous rewinding and slitting performance for demanding research and production workflows.
300mm Small Laboratory Automatic Roll to Roll Coating Machine
Improve lithium battery electrode prototyping with a 300mm small laboratory automatic roll to roll coating machine featuring precision doctor blade coating hot air drying and automatic web guiding for uniform experimental electrode production in materials laboratories and pilot lines.
Four Sided Multi Groove Film Applicator for Coin Cell Laboratory Research
Four-sided multi-groove film applicator for coin cell laboratory research enables uniform coating of paints binders and electrode slurries across selectable wet film thicknesses using durable stainless steel construction for repeatable manual sample preparation in battery materials and laboratory workflows.
Doctor Blade Continuous Coating Machine for Battery Electrode Sheets
Doctor blade continuous coating machine delivers precision electrode films with stable web tension, dual-sided hot-air drying, PLC operation, and accurate alignment for lithium-ion batteries, supercapacitors, nickel batteries, pilot-scale development, and advanced materials research.
Automatic Large Area Laboratory Hot Press Laminator 15 Ton 500x500mm Heated Platens Data Logging CE Certified
Automatic large-area laboratory hot press laminator with 500x500mm heated platens, 15-ton force, programmable PID control, data logging and USB export, CE certified. Designed for composites, PCBs, flexible electronics. Ensure reproducibility in your lamination processes. Ideal for research and pilot production.
Laboratory Heated Horizontal Double Roll Machine with Dual Servo Motors
Laboratory heated horizontal double roll machine with dual servo motors delivers adjustable thickness, accurate speed control, and digital heating for consistent battery electrode rolling and advanced materials processing in compact research laboratories and pilot scale development environments applications
Manual Heated Hydraulic Press 300x300mm Platen 40 Ton Force 4.4 MPa Independent Dual Zone PID Temp Control
Manual heated hydraulic press with 300x300 mm platen, 40-ton force, 4.4 MPa, independent dual-zone PID temperature control to 300°C. Ideal for polymer film, composite, and flexible device lamination. Request a quote.
Slot Die Extrusion Coating Machine for Roll to Roll Electrode Coating
Slot die extrusion coating machine delivers non-contact roll-to-roll electrode coating with precision syringe pumping, controlled infrared drying, and glovebox-ready compact operation for solid-state battery, functional film, and laboratory process development where repeatable coating, web tracking, and temperature uniformity support results.
Benchtop Automatic Vacuum Hot Press for Advanced Material Processing
High-precision benchtop automatic vacuum hot press delivering 25 tons of force, dual large-area heated platens up to 300°C, oil-free clean vacuum, programmable multi-stage pressing for repeatable results. Perfect for solid-state battery fabrication, polymer film lamination, and advanced material development.
20 Ton 500x500mm Split-Type Automatic Hot Press with Programmable PID Temperature Control
Professional 20-ton split-type hot press with 500x500mm platen, 7kW PID-controlled heating up to 300°C, and automatic pressure regulation. Ideal for polymer pressing, composite lamination, and battery electrode fabrication in lab or pilot environments. Robust split design ensures long-term reliability.
Heated Roll to Roll Roller Press Battery Electrode Two Roll Mill Laboratory Two Roll Mill
Heated laboratory roll to roll roller press for battery electrode calendering and nonferrous materials with adjustable gap independent heating digital temperature control and continuous web handling for repeatable research scale processing and dense electrode development in advanced laboratories