Products Battery Testing & Electrochemical Equipment In-situ Raman Test Cell Quick Change Zinc Plate Large Capacity Zinc Air Test Cell
Toggle Categories
Quick Change Zinc Plate Large Capacity Zinc Air Test Cell

In-situ Raman Test Cell

Quick Change Zinc Plate Large Capacity Zinc Air Test Cell

Item Number : BE02

Price varies based on specs and customizations


Liquid Capacity
30 ml
Reaction Area
1 cm², 2 cm², 3 cm², 4 cm², or 5 cm²
Positive-to-Negative Electrode Distance
0.5 cm
ISO & CE icon

Shipping:

Contact us to get shipping details Enjoy On-time Dispatch Guarantee.

View Specs

Why Choose Us

Easy ordering process, quality products, and dedicated support for your business success.

Easy Process Quality Assured Dedicated Support

Product Overview

Product image 1

Product image 3

This quick change zinc air test cell is designed for laboratory evaluation of zinc air battery chemistries and zinc electrode performance. Its plug-in anode fixture allows a zinc plate to be removed and replaced in approximately 2 seconds, reducing interruption between experiments and supporting efficient comparative testing. The transparent PMMA housing provides direct visibility of the internal assembly and electrolyte condition during operation.

The unit provides a 30 ml liquid capacity, allowing the assembled cell to sustain extended electrochemical reactions without frequent manual replenishment. Multiple reaction-area configurations support different experimental requirements, while the 0.5 cm electrode spacing establishes a consistent test geometry. This equipment is suited to battery R&D, electrochemical materials development, academic research, and laboratory-scale zinc air cell investigation.

Built for repeated controlled testing, the equipment combines a durable transparent enclosure with a straightforward manually operated configuration. The fixed anode structure helps maintain repeatable positioning, while the visible housing makes it easier to monitor the cell during assembly and operation. Proper PMMA handling and manual liquid addition are required for reliable long-term use.

Key Features

  • Rapid Plug-In Anode Replacement: The fixed plug-in anode structure enables zinc plates to be changed in approximately 2 seconds, supporting fast sample comparison and reducing downtime between tests.

  • Transparent PMMA Housing: The organic glass enclosure is transparent and durable, allowing researchers to observe the internal cell structure, electrode arrangement, and liquid condition without disassembling the unit.

  • 30 ml Liquid Capacity: The cell accommodates 30 ml of liquid, helping maintain extended battery reactions after assembly and reducing the need for frequent manual electrolyte addition.

  • Consistent Electrode Geometry: A 0.5 cm positive-to-negative electrode distance provides a defined spacing arrangement for repeatable zinc air battery experiments and controlled laboratory comparisons.

  • Multiple Reaction Areas: Configurations with reaction areas of 1, 2, 3, 4, or 5 cm² allow researchers to select a test format suited to the active electrode area and experimental objective.

  • Compatible Zinc Plate Dimensions: The anode fixture accepts zinc plates up to 34 mm wide, up to 2.5 mm thick, and between 55 and 80 mm long, providing practical flexibility for electrode preparation.

  • Compact Laboratory Format: Measuring 6.5 by 6 by 7.2 cm, the equipment uses limited bench space and can be integrated into laboratory workflows for battery materials screening and electrochemical testing.

  • Manual Liquid Addition: The simple manually filled design supports direct control over liquid addition during experiments. It is intended for manual operation and is not compatible with circulation pumps.

Applications

Application Description Key Benefit
Zinc Air Battery Research Evaluate zinc plate anodes, air cathode assemblies, and electrolyte behavior in laboratory-scale zinc air battery experiments. Rapid electrode replacement accelerates sample comparison and screening.
Zinc Electrode Material Evaluation Compare zinc plate compositions, surface treatments, thicknesses, and preparation methods within a defined cell geometry. Consistent 0.5 cm electrode spacing improves test-to-test comparability.
Electrolyte Formulation Studies Investigate the influence of different manually added liquid formulations on zinc air cell reaction behavior. The 30 ml capacity supports longer reactions with fewer interruptions.
Battery R&D Laboratories Support early-stage cell design, electrode validation, and performance experiments before larger-format development. Compact dimensions conserve bench space while providing several reaction-area choices.
Academic Electrochemistry Research Provide a visible test platform for teaching, research, and repeatable demonstrations involving zinc air electrochemistry. Transparent PMMA construction makes internal conditions easier to observe.
Advanced Materials Development Examine how new electrode or electrolyte materials perform in a controlled zinc air test configuration. Quick anode changes improve experimental throughput during material screening.
Small-Scale Cell Assembly Studies Assemble and assess laboratory battery structures using zinc plates within specified dimensional limits. The fixed anode fixture simplifies positioning and replacement.

Technical Specifications

Parameter Specification Notes
Product item number BE02 Site-facing identifier for this product
Site-facing variant identifiers BE02 1 cm², BE02 2 cm², BE02 3 cm², BE02 4 cm², BE02 5 cm² Identifiers are differentiated by reaction area
Mold material Organic glass PMMA Transparent and durable housing material
Overall dimensions 6.5 × 6 × 7.2 cm Length × width × height
Positive-to-negative electrode distance 0.5 cm Fixed electrode spacing
Reaction area variants 1 cm², 2 cm², 3 cm², 4 cm², 5 cm² Selectable configuration range
Liquid capacity 30 ml Capacity after assembly for sustained reaction testing
Compatible anode width ≤34 mm Zinc plate requirement
Compatible anode thickness ≤2.5 mm Zinc plate requirement
Compatible anode length 55 mm to 80 mm Zinc plate requirement
Anode replacement method Plug-in fixed anode structure Replacement can be completed within approximately 2 seconds
Liquid addition method Manual liquid addition only Not suitable for circulation pumps
PMMA cleaning restriction Do not place the PMMA plate directly in alcohol solution or pour alcohol onto its surface Alcohol exposure can cause surface cracking or damage
PMMA surface cleaning guidance When oil is present, use a tissue lightly moistened with a small amount of alcohol to clean the surface Apply alcohol sparingly and indirectly
Ultrasonic cleaning Prohibited Do not use ultrasonic cleaning on the PMMA plate

The five reaction-area configurations provide practical flexibility for experiments using different active electrode sizes. The corresponding site-facing identifiers are based on the product item number and the documented reaction-area differentiator: BE02 1 cm², BE02 2 cm², BE02 3 cm², BE02 4 cm², and BE02 5 cm². No unsupported performance values, operating temperatures, pressure ratings, or automated circulation functions are specified for this equipment.

For correct operation, users should prepare zinc plates within the documented dimensional limits and install them in the plug-in anode fixture. The rapid replacement mechanism is intended to simplify manual laboratory workflows, but the electrode must still be positioned correctly before each reaction. The 30 ml liquid capacity is available after assembly, and liquid addition must be performed manually because the configuration is not designed for a circulation pump.

PMMA care is important for maintaining enclosure clarity and structural condition. The plate must not be immersed directly in alcohol or have alcohol poured over its surface. If oil contamination occurs, a tissue containing only a small amount of alcohol may be used to wipe the surface. Ultrasonic cleaning is prohibited because it may damage the PMMA component. Following these handling requirements helps preserve visibility for ongoing observation and supports consistent use across repeated experiments.

Why Choose This Product

  • Efficient Experimental Turnaround: Approximately 2-second anode replacement supports faster zinc plate screening and reduces handling time between laboratory tests.

  • Visible Internal Test Environment: Transparent PMMA construction allows direct observation of the cell, helping researchers inspect assembly and liquid conditions during operation.

  • Flexible Research Configuration: Five documented reaction-area options accommodate different electrode test formats without requiring a separate basic cell architecture for every experiment.

  • Controlled, Repeatable Geometry: Fixed anode positioning and a defined 0.5 cm electrode distance provide a consistent foundation for comparative zinc air battery studies.

  • Practical Long-Duration Testing: The 30 ml liquid capacity supports sustained reactions while the compact format fits efficiently into laboratory battery and materials research workflows.

Choose a configuration matched to your reaction area and zinc plate dimensions, then contact us for a quotation or a laboratory solution aligned with your testing requirements.

Trusted by Industry Leaders

Our Cooperated Clients
View more faqs for this product

Product Datasheet

Quick Change Zinc Plate Large Capacity Zinc Air Test Cell

Category Catalog

In-Situ Raman Test Cell


REQUEST A QUOTE

Our professional team will reply to you within one business day. Please feel free to contact us!

Related Products

Automatic Large Area Laboratory Hot Press Laminator 15 Ton 500x500mm Heated Platens Data Logging CE Certified

Automatic Large Area Laboratory Hot Press Laminator 15 Ton 500x500mm Heated Platens Data Logging CE Certified

Automatic large-area laboratory hot press laminator with 500x500mm heated platens, 15-ton force, programmable PID control, data logging and USB export, CE certified. Designed for composites, PCBs, flexible electronics. Ensure reproducibility in your lamination processes. Ideal for research and pilot production.

View Details
Automatic High Pressure Hot Press 90 Ton 300x300mm Platens 0.2% Pressure Accuracy 200C

Automatic High Pressure Hot Press 90 Ton 300x300mm Platens 0.2% Pressure Accuracy 200C

Discover the automatic high-pressure hot press delivering 90 tons of force on 300×300 mm platens with 0.2% pressure accuracy and precise PID temperature control up to 200°C, ideal for battery research, semiconductor packaging, polymer molding, and composite densification.

View Details
Lab Double Plate Heating Mold for Laboratory Use

Lab Double Plate Heating Mold for Laboratory Use

Precision Double Plate Heating Mold for labs, featuring dual-zone temperature control, rapid cooling, and uniform heating. Ideal for material testing and sample preparation.

View Details
Desktop Continuous Film Coating Testing Machine for 18650 Cylindrical Batteries

Desktop Continuous Film Coating Testing Machine for 18650 Cylindrical Batteries

Desktop continuous coating machine for lithium battery electrodes 18650 cylindrical cell research ceramic films crystal films and nanofilms offering adjustable coating width precise thickness control automatic rewinding and independent PID oven temperature regulation for university laboratories and small scale production

View Details
30 Ton Split Type Automatic Lab Hot Press with 300x300mm Heated Platens and PID Control

30 Ton Split Type Automatic Lab Hot Press with 300x300mm Heated Platens and PID Control

30-ton split-type automatic laboratory hot press with 300x300mm heated platens, PID temperature and pressure control, 5-step programmable recipes, water cooling, dual-zone independent heating. Standard 300°C and high-temperature 500°C versions available. Ideal for battery research and precise sample preparation. CE certified.

View Details
Lab Cylindrical Press Mold for Laboratory Use

Lab Cylindrical Press Mold for Laboratory Use

Precision cylindrical press molds for lab sample prep. Durable, high-performance, and customizable for XRF, battery research, and material testing. Get yours today!

View Details
Integrated Manual Heated Plate Hydraulic Press for Laboratory

Integrated Manual Heated Plate Hydraulic Press for Laboratory

The integrated manual heated plate lab press provides 0-40 tons, 300°C, 200x200mm platens, 7-inch touchscreen, and water cooling. Perfect for polymers, ceramics, and battery research. Achieve precise, consistent sample preparation with advanced over-temperature protection. Request a quote today.

View Details
Lab Button Battery Disassembly and Sealing Mold

Lab Button Battery Disassembly and Sealing Mold

KINTEK's precision button battery sealing molds ensure airtight, contamination-free results for labs and production. Boost efficiency with durable, high-performance solutions.

View Details